The simultaneous synthesis and densification of rhenium diboride is investigated starting from Re and B as reactants by using the Spark Plasma Sintering (SPS) apparatus. It is shown that SPS represents an effective technique to synthesize ReB(2) bulk samples with high purity and density. In particular, a dense product with traces of secondary phases (Re(7)B(3)) is obtained in 35 min of total processing time by applying a maximum temperature of 1600 degrees C and a mechanical pressure of 20 MPa. (C) 2008 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Reactive Spark Plasma Sintering of rhenium diboride

LOCCI, ANTONIO MARIO;LICHERI, ROBERTA;ORRU', ROBERTO;CAO, GIACOMO
2009-01-01

Abstract

The simultaneous synthesis and densification of rhenium diboride is investigated starting from Re and B as reactants by using the Spark Plasma Sintering (SPS) apparatus. It is shown that SPS represents an effective technique to synthesize ReB(2) bulk samples with high purity and density. In particular, a dense product with traces of secondary phases (Re(7)B(3)) is obtained in 35 min of total processing time by applying a maximum temperature of 1600 degrees C and a mechanical pressure of 20 MPa. (C) 2008 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11584/100967
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 50
  • ???jsp.display-item.citation.isi??? 46
social impact