We study by scanning thermal microscopy the nanoscale thermal conductance of films (40-400 nm thick) of [1]benzothieno[3,2-b][1]benzothiophene (BTBT) and 2,7-dioctyl[1]benzothieno[3,2-b][1]benzothiophene (C8-BTBT-C8). We demonstrate that the out-of-plane thermal conductivity is significant along the interlayer direction, larger for BTBT (0.63 ± 0.12 W m-1 K-1) compared to C8-BTBT-C8 (0.25 ± 0.13 W m-1 K-1). These results are supported by molecular dynamics calculations (approach to equilibrium molecular dynamics method) performed on the corresponding molecular crystals. The calculations point to significant thermal conductivity (3D-like) values along the 3 crystalline directions, with anisotropy factors between the crystalline directions below 1.8 for BTBT and below 2.8 for C8-BTBT-C8, in deep contrast with the charge transport properties featuring a two-dimensional character for these materials. In agreement with the experiments, the calculations yield larger values in BTBT compared to C8-BTBT-C8 (0.6-1.3 W m-1 K-1versus 0.3-0.7 W m-1 K-1, respectively). The weak thickness dependence of the nanoscale thermal resistance is in agreement with a simple analytical model.

Thermal conductivity of benzothieno-benzothiophene derivatives at the nanoscale

Lenfant S.
Membro del Collaboration Group
;
Antidormi A.
Membro del Collaboration Group
;
Melis C.
Membro del Collaboration Group
;
2021-01-01

Abstract

We study by scanning thermal microscopy the nanoscale thermal conductance of films (40-400 nm thick) of [1]benzothieno[3,2-b][1]benzothiophene (BTBT) and 2,7-dioctyl[1]benzothieno[3,2-b][1]benzothiophene (C8-BTBT-C8). We demonstrate that the out-of-plane thermal conductivity is significant along the interlayer direction, larger for BTBT (0.63 ± 0.12 W m-1 K-1) compared to C8-BTBT-C8 (0.25 ± 0.13 W m-1 K-1). These results are supported by molecular dynamics calculations (approach to equilibrium molecular dynamics method) performed on the corresponding molecular crystals. The calculations point to significant thermal conductivity (3D-like) values along the 3 crystalline directions, with anisotropy factors between the crystalline directions below 1.8 for BTBT and below 2.8 for C8-BTBT-C8, in deep contrast with the charge transport properties featuring a two-dimensional character for these materials. In agreement with the experiments, the calculations yield larger values in BTBT compared to C8-BTBT-C8 (0.6-1.3 W m-1 K-1versus 0.3-0.7 W m-1 K-1, respectively). The weak thickness dependence of the nanoscale thermal resistance is in agreement with a simple analytical model.
File in questo prodotto:
File Dimensione Formato  
cmelis-nanoscale.pdf

Open Access dal 05/02/2022

Descrizione: Articolo principale
Tipologia: versione post-print (AAM)
Dimensione 2.47 MB
Formato Adobe PDF
2.47 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11584/325853
Citazioni
  • ???jsp.display-item.citation.pmc??? 3
  • Scopus 16
  • ???jsp.display-item.citation.isi??? 16
social impact