Dense (Zr0.5Hf0.5)B2–SiC composites were produced in this work using three different approaches: (a) coupling Self-propagating High-temperature Synthesis (SHS) and Spark Plasma Sintering (SPS) techniques (SHS-SPS) from Hf, Zr, Si, B, and B4C reactants; (b) Reactive SPS (RSPS) using the same precursors as in (a); and (c) adding commercial (ex-situ) SiC particles prior to SPS into diboride powders prepared by SHS. In-situ SHS-SPS processing required, in the presence of SiC, a lower sintering temperature (1750°C) compared to alternative routes (1850°C) to obtain the equimolar diboride as a single phase. This approach was also found to optimally incorporate SiC into the ceramic matrix. Moreover, unlike RSPS and the use of ex-situ produced SiC, this method also yielded finer and more uniform microstructures, which maximized fracture toughness and enhanced oxidation resistance. In particular, after exposure for 1 h in an air furnace at 1400 °C, the specific mass gain of the samples was significantly reduced in the presence of SiC, dropping from 5.9 to 0.7 mg/cm². In parallel, the thickness of the generated oxide scale decreased markedly from about 140–15 μm. This behavior is directly attributable to the formation of a protective borosilicate phase, whose surface coverage of the samples improves with increasing SiC content.

How in-situ SiC formation impacts the sintering behavior, phase evolution, oxidation resistance, and mechanical properties of (Zr0.5Hf0.5)B2–SiC composites

Casu, Mariano
Primo
;
Cappai, Luca;Pakhomova, Ekaterina;Licheri, Roberta;Locci, Antonio Mario;Cao, Giacomo;Orru', Roberto
Ultimo
2026-01-01

Abstract

Dense (Zr0.5Hf0.5)B2–SiC composites were produced in this work using three different approaches: (a) coupling Self-propagating High-temperature Synthesis (SHS) and Spark Plasma Sintering (SPS) techniques (SHS-SPS) from Hf, Zr, Si, B, and B4C reactants; (b) Reactive SPS (RSPS) using the same precursors as in (a); and (c) adding commercial (ex-situ) SiC particles prior to SPS into diboride powders prepared by SHS. In-situ SHS-SPS processing required, in the presence of SiC, a lower sintering temperature (1750°C) compared to alternative routes (1850°C) to obtain the equimolar diboride as a single phase. This approach was also found to optimally incorporate SiC into the ceramic matrix. Moreover, unlike RSPS and the use of ex-situ produced SiC, this method also yielded finer and more uniform microstructures, which maximized fracture toughness and enhanced oxidation resistance. In particular, after exposure for 1 h in an air furnace at 1400 °C, the specific mass gain of the samples was significantly reduced in the presence of SiC, dropping from 5.9 to 0.7 mg/cm². In parallel, the thickness of the generated oxide scale decreased markedly from about 140–15 μm. This behavior is directly attributable to the formation of a protective borosilicate phase, whose surface coverage of the samples improves with increasing SiC content.
2026
(Zr,Hf)B2; Oxidation behaviour; SiC, In-situ synthesis; Spark plasma sintering
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I metadati presenti in IRIS UNICA sono rilasciati con licenza Creative Commons CC0 1.0 Universal, mentre i file delle pubblicazioni sono protetti da diritto d'autore, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11584/497545
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
  • OpenAlex ND
social impact